The Causes Of Twelve Injection Molding Defects Are Perfectly Analyzed In 360 Degree Depth
Sep 30, 2018

I. analysis of causes of cracking of injection molded products

2. Cause analysis of bubble in injection molded products

3.Analysis of causes of warping deformation of injection molded products

4.Analysis of color pattern of color line of injection molded products

5.Cause analysis of shrinkage sag of injection molded parts

6.Cause analysis of transparent defect of injection molded products

7.Cause analysis of color imbalance of injection molded products

8.Cause analysis of silver inlay in injection molded products

9.Analysis on the causes of weld penetration in plastic products

10.Analysis on the cause of shock grain of injection molded products

11.Analysis of causes of swelling and bubbling of injection molded products